4150 Dybar is a special quality alloy steel that has been resulphurized for considerations for machining. Modifications have been made to the chemical composition for increased hardenability. This steel is made by a single slab electric furnace process to a silicon fully killed practice and resulphurized to set limits.
|
TYPICAL ANALYSIS |
AISI 4150 |
|
Carbon (C) |
.47/.55 |
|
Manganese (Mn) |
.95/1.30 |
|
Silicon (Si) |
.20/.35 |
|
Molybdenum (Mo) |
.15/.25 |
|
Chromium (Cr) |
.60/.90 |
|
Vanadium (V) |
.10 MAX |
|
Sulphur (S) |
.06/.10 |
|
Phosphorus (P) |
.025 MAX |
|
Nickel (Ni) |
.25 MAX |
|
Columbium |
.015/.035 |
|